Free chart · Sourced from the makers

Filament drying chart Every maker’s numbers, side by side.

Drying temperature and time for 14 filament types, with print temperatures, from 17 manufacturers’ own pages. Where makers disagree, you see the whole range and its sources, not one invented number.

  • Sourced172 values, each linked
  • The spreadWhere makers disagree
  • 14 materialsFrom PLA to PEEK
  • Your dryerSee what it can reach
Material

Shows which settings your dryer can reach.

PLA, PLA+ and silk PLA

Dry PLA at 50 °C

for 5–6 hours, what most makers publish. Makers range from 40 to 65 °C, a wide spread: follow the maker of your spool.

Time, all makers
0–12 h
Nozzle
190–230 °C
Bed
45–60 °C
Enclosure
Not needed (7 of 7 makers)
PLA, PLA+ and silk PLA: drying and print settings published by 16 makers
MakerDrying 40–70 °C scaleTimeMethodNozzleBedSource
AnycubicAnycubic’s blog gives 40–45 °C for PLA. 40–45 °C4–6 h———Anycubic Store blog
FormfuturaTransparent PLA 40–50 °C4–6 h—190–225 °C45–55 °CFormFutura
Siraya Tech 40–45 °C max4–6 h———Siraya Tech blog
AnycubicAnycubic PLA BasicAnycubic’s blog gives 40–45 °C for PLA. 45–50 °C6–8 h—190–230 °C—Anycubic
Formfutura 45–55 °C4–6 h———FormFutura blog
PrusaPrusament PLA / rPLA 45 °C6 h—200–220 °C40–60 °CPrusa Knowledge BasePrint temperatures: Prusament (Prusa Research)
Bambu LabPLA Basic / PLA Matte 50 °C8 hForced-air ovenPrinter’s heated bed: 60–70 °C, 12 hAMS 2 Pro: 45 °C, 12 hAMS HT: 45 °C, 12 h190–240 °C45–65 °CBambu Lab WikiPrint temperatures: Bambu Lab Wiki
colorFabbPLA Economy 50 °C4 h—195–220 °C50–60 °CcolorFabb
eSUNPLA series 50 °C————eSUN Wiki
eSUNeSUN PLA Basic 50 °C8–12 h—210–230 °C45–60 °CeSUN
ExtrudrPLA High-Speed 50 °C0–6 h——20–60 °CExtrudr
FillamentumPLA Extrafill 50 °C max3 hLaboratory dryer——Fillamentum
FillamentumPLA Crystal Clear 50 °C4 hLaboratory dryer——Fillamentum
Flashforge 50 °C4–6 h———Flashforge Wiki
FlashforgeFlashforge HS PLA 50 °C5 hConvection oven190–240 °C25–60 °CFlashforge
MatterHackers 50 °C4 hFilament dryer——MatterHackers
Overture 50 °C7 h———Overture 3D Wiki
SUNLUSUNLU PLA 50 °C——185–230 °C50–60 °CSUNLU
SUNLUSUNLU PLA+PLA+ / tough PLA 50 °C——205–245 °C50–60 °CSUNLU
SUNLUSUNLU Silk PLA+Silk PLA 50 °C——210–230 °C50–60 °CSUNLU
Bambu LabPLA SilkSilk PLA 55 °C8 hForced-air ovenPrinter’s heated bed: 65–75 °C, 12 hAMS 2 Pro: 45 °C, 12 hAMS HT: 45 °C, 12 h190–240 °C45–65 °CBambu Lab WikiPrint temperatures: Bambu Lab Wiki
CrealityCR-PLA (print temps) 55 °C8–12 hFilament dryer190–230 °C—Creality Store blogPrint temperatures: Creality Store blog
PolymakerPolyLite PLA 55 °C6 h—190–230 °C25–60 °CPolymaker Wiki
PolymakerPanchroma Silk PLASilk PLA 55 °C6 h—190–230 °C25–60 °CPolymaker Wiki
colorFabbPLA HPPLA+ / tough PLA 60 °C6 h—200–220 °C50–60 °CcolorFabb
3DXTech 65 °C max4 hOven——3DXTECH

Shaded: what most makers publish. Hollow: published as a maximum, not a target. Typical print temperatures are the middle of what makers publish.

PETG and other copolyesters

Dry PETG at 60–65 °C

for 6 hours, what most makers publish. Makers range from 50 to 70 °C, a wide spread: follow the maker of your spool.

Time, all makers
0–12 h
Nozzle
230–260 °C
Bed
60–80 °C
Enclosure
Recommended by 1 of 5 makers

Shaded: what most makers publish. Hollow: published as a maximum, not a target. Typical print temperatures are the middle of what makers publish.

ABS

Dry ABS at 70–80 °C

for 5–6 hours, what most makers publish. Makers range from 60 to 85 °C, a wide spread: follow the maker of your spool.

Time, all makers
2–12 h
Nozzle
240–265 °C
Bed
90–100 °C
Enclosure
Recommended by 4 of 4 makers

Shaded: what most makers publish. Hollow: published as a maximum, not a target. Typical print temperatures are the middle of what makers publish.

ASA and ASA-CF

Dry ASA at 75–80 °C

for 7 hours, what most makers publish. Makers range from 60 to 85 °C, a wide spread: follow the maker of your spool.

Time, all makers
2–12 h
Nozzle
240–270 °C
Bed
90–105 °C
Enclosure
Recommended by 6 of 6 makers

Shaded: what most makers publish. Hollow: published as a maximum, not a target. Typical print temperatures are the middle of what makers publish.

TPU and other flexibles

Dry TPU at 65–70 °C

for 6 hours, what most makers publish. Makers range from 45 to 100 °C, a wide spread: follow the maker of your spool.

Time, all makers
3–24 h
Nozzle
215–240 °C
Bed
40–60 °C
Enclosure
Not needed (9 of 9 makers)

Shaded: what most makers publish. Hollow: published as a maximum, not a target. Typical print temperatures are the middle of what makers publish.

Nylon (PA6, PA12, PAHT)

Dry Nylon at 80–85 °C

for 8 hours, what most makers publish. Makers range from 65 to 125 °C, a wide spread: follow the maker of your spool.

Time, all makers
3–12 h
Nozzle
250–280 °C
Bed
80–90 °C
Enclosure
Recommended by 4 of 5 makers

Shaded: what most makers publish. Hollow: published as a maximum, not a target. Typical print temperatures are the middle of what makers publish.

Polycarbonate and PC-CF

Dry PC at 75–80 °C

for 6 hours, what most makers publish. Makers range from 65 to 120 °C, a wide spread: follow the maker of your spool.

Time, all makers
2–24 h
Nozzle
260–290 °C
Bed
100–120 °C
Enclosure
Recommended by 6 of 8 makers

Shaded: what most makers publish. Hollow: published as a maximum, not a target. Typical print temperatures are the middle of what makers publish.

Carbon-fibre PLA

Dry PLA-CF at 55 °C

for 7 hours, what most makers publish. Makers range from 50 to 60 °C.

Time, all makers
6–12 h
Nozzle
200–235 °C
Bed
50–60 °C
Enclosure
Not needed (2 of 2 makers)

Shaded: what most makers publish. Hollow: published as a maximum, not a target. Typical print temperatures are the middle of what makers publish.

Carbon-fibre PETG and PET

Dry PETG-CF at 70 °C

for 7 hours, what most makers publish. Makers range from 60 to 90 °C, a wide spread: follow the maker of your spool.

Time, all makers
4–12 h
Nozzle
240–265 °C
Bed
60–80 °C
Enclosure
Recommended by 1 of 1 makers

Shaded: what most makers publish. Hollow: published as a maximum, not a target. Typical print temperatures are the middle of what makers publish.

Carbon-fibre nylon

Dry PA-CF at 80–90 °C

for 7–8 hours, what most makers publish. Makers range from 65 to 125 °C, a wide spread: follow the maker of your spool.

Time, all makers
4–12 h
Nozzle
260–290 °C
Bed
90–110 °C
Enclosure
Recommended by 4 of 6 makers

Shaded: what most makers publish. Hollow: published as a maximum, not a target. Typical print temperatures are the middle of what makers publish.

PVA (water-soluble support)

Dry PVA at 65–70 °C

for 7–8 hours, what most makers publish. Makers range from 45 to 85 °C, a wide spread: follow the maker of your spool.

Time, all makers
6–12 h
Nozzle
190–240 °C
Bed
45–65 °C
Enclosure
Not needed (1 of 1 makers)

Shaded: what most makers publish. Hollow: published as a maximum, not a target. Typical print temperatures are the middle of what makers publish.

HIPS (support)

Dry HIPS at 75 °C

for 3 hours, what most makers publish. Makers range from 70 to 80 °C.

Time, all makers
3–6 h
Nozzle
—
Bed
—
Enclosure
Not stated

Shaded: what most makers publish. Hollow: published as a maximum, not a target. Typical print temperatures are the middle of what makers publish.

Polypropylene

Dry PP at 65 °C

for 2–3 hours, what most makers publish. Makers range from 50 to 80 °C, a wide spread: follow the maker of your spool.

Time, all makers
2–4 h
Nozzle
235–255 °C
Bed
65–80 °C
Enclosure
Not needed (1 of 1 makers)

Shaded: what most makers publish. Hollow: published as a maximum, not a target. Typical print temperatures are the middle of what makers publish.

PEEK and PEI

Dry PEEK / PEI at 120 °C

for 4 hours, what most makers publish. Makers range from 70 to 150 °C, a wide spread: follow the maker of your spool.

Time, all makers
4–8 h
Nozzle
395–420 °C
Bed
125–140 °C
Enclosure
Recommended by 2 of 2 makers

Shaded: what most makers publish. Hollow: published as a maximum, not a target. Typical print temperatures are the middle of what makers publish.

Advertisement

At a glance

The filament drying chart

What most makers publish for each material, and the full range between them. Choose a material in the chart above to see every maker’s figure and its source.

MaterialDrying (most makers)Makers’ rangeTimeNozzleBedMakers
50 °C40–65 °C5–6 h190–230 °C45–60 °C16
60–65 °C50–70 °C6 h230–260 °C60–80 °C17
70–80 °C60–85 °C5–6 h240–265 °C90–100 °C13
75–80 °C60–85 °C7 h240–270 °C90–105 °C14
65–70 °C45–100 °C6 h215–240 °C40–60 °C14
80–85 °C65–125 °C8 h250–280 °C80–90 °C15
75–80 °C65–120 °C6 h260–290 °C100–120 °C11
55 °C50–60 °C7 h200–235 °C50–60 °C5
70 °C60–90 °C7 h240–265 °C60–80 °C8
80–90 °C65–125 °C7–8 h260–290 °C90–110 °C10
65–70 °C45–85 °C7–8 h190–240 °C45–65 °C4
75 °C70–80 °C3 h——4
65 °C50–80 °C2–3 h235–255 °C65–80 °C4
120 °C70–150 °C4 h395–420 °C125–140 °C3

“Most makers” is the middle of the published values: half the makers publish more, half less. Print temperatures are the middle of each maker’s published range.

Why charts disagree

Where makers disagree, and what to do

Makers test their own resin blends, spools and dryers, so their numbers differ. The widest spreads:

  • TPU: from 45 °C (Siraya Tech’s blog) to 100 °C (Fillamentum TPU 98A). Softer grades are not always dried cooler.
  • Nylon: from 65 °C (Extrudr PA12) to 125 °C (colorFabb). Fillamentum warns against going above 80 °C, because nylon can oxidise.
  • PC: from 65 °C to a 120 °C maximum, and from 2 to 24 hours.
  • PVA: from 45 °C to 85 °C. Bambu Lab’s own material table and drying page disagree.

Some makers contradict themselves: Bambu Lab’s material table and its drying page give different PLA, PETG and PVA figures, and Overture’s wiki and blog differ for PETG. Where a page gives two values, the chart shows the main one and says so.

What to do: follow the maker of your spool. If it publishes nothing, start at the low end of what most makers publish and dry longer rather than hotter.

Method

How to dry filament safely

  1. Use a dryer or an oven you can trust. Many makers specify a forced-air (blast) oven. Kitchen ovens often overshoot their setting, so check with a separate thermometer.
  2. Stay at or below the maker’s temperature. Above it, filament can soften and stick to itself, and the spool can warp. Several makers publish their figure as a maximum.
  3. Check the spool. Prusa notes that older black Prusament spools only handle 45 °C. Cardboard spools are safer than thin plastic in an oven.
  4. Dry for the full time, then print from a dry box or seal the spool with desiccant.

Printers with drying modes (such as Bambu Lab’s AMS 2 Pro and AMS HT, or drying on the heated bed) use lower temperatures for longer. Those figures appear under the method where makers publish them.

Moisture

Signs your filament needs drying

  • Popping or hissing at the nozzle, and steam from the extrudate.
  • Stringing and oozing that weren’t there with a new spool.
  • Rough, bubbly or dull surfaces, and weak layers that snap easily.
  • Brittle filament that breaks in the feed path (common with PLA and PVA).

Several makers, Polymaker among them, recommend printing moisture-sensitive materials such as PC and nylon straight from a dry box or dryer.

Questions, answered

What temperature should I dry PLA at?

Most makers publish 50 °C for 5–6 hours. Some go lower (Anycubic and Siraya Tech give 40–45 °C), and Fillamentum says PLA should not go above 50 °C. Follow your spool’s maker.

Can I dry filament in a kitchen oven?

It works if the oven holds a low temperature steadily, but many overshoot. Check with a separate thermometer, and never leave plastic unattended in an oven.

Is it bad to dry filament too long?

For most materials, longer at the right temperature is safe. Nylon is the exception: 3DXTech notes that over-drying can make it brittle.

Why are some values shown as a maximum?

Some makers (such as 3DXTech) publish the highest temperature the filament and spool can take, not a target. Drying a little below it is fine.

Where do these numbers come from?

Every value was read on the maker’s own page, data sheet or wiki on 2026-11-08, and each row links to it. We don’t average or invent missing values; a dash means the maker doesn’t publish one.

Sources

Print advice is a starting point drawn from these references, checked on 2026-11-08. Community posts are one maker's experience, not a specification.

  1. Filament Drying Recommendations 3DXTECH
  2. Anycubic PLA Basic filament Anycubic
  3. Anycubic PETG Filament Anycubic
  4. Anycubic PET-CF Filament Anycubic
  5. How to Dry Wet 3D Printer Filament - Simple and Easy Ways (2024-01-04) Anycubic Store blog
  6. Filament Drying Recommendations Bambu Lab Wiki
  7. Filament guide - Printer, Nozzle, AMS, Build Plate, Glue Compatibility and Required Parameters Bambu Lab Wiki
  8. colorFabb Print Support (print & drying settings table) colorFabb
  9. Filament Dryer Temperature and Time Chart for PLA, PETG, TPU, ABS, ASA and Nylon (2026-08-14) Creality Store blog
  10. Creality Filaments' Parameter Reference Table (2024-12-23) Creality Store blog
  11. Rapid PETG ELEGOO
  12. ELEGOO PETG PRO Filament ELEGOO
  13. ELEGOO PETG-CF ELEGOO
  14. ELEGOO PAHT-CF ELEGOO
  15. eSUN PETG Filament TDS (JUL.2025 Version 2.0) eSUN
  16. eSUN PLA-Basic TDS (Feb.2026 Version1.0) eSUN
  17. 3D Printing Filament Drying Temperatures Guide (FAQ: Drying temperatures) eSUN Wiki
  18. PLA High-Speed Extrudr
  19. PETG Filament Extrudr
  20. XPETG CF Filament Extrudr
  21. DuraPro ABS Filament Extrudr
  22. DuraPro ASA Filament Extrudr
  23. DuraPro PA12 Extrudr
  24. DuraPro PA12 CF Extrudr
  25. DuraPro PC/PBT Filament Extrudr
  26. TPU FLEX Semisoft Extrudr
  27. TPU FLEX Medium Extrudr
  28. Recommendation for processing: Drying of filaments before processing on 3D printer (rev. 12 Oct 2023) Fillamentum
  29. HS PLA Filament Flashforge
  30. HS PETG Flashforge
  31. Drying Temperature and Time for Common Filaments Flashforge Wiki
  32. Transparent PLA FormFutura
  33. Python Flex TPU 90A FormFutura
  34. Technical Data Sheet ReForm rTPU 95A FormFutura
  35. Technical Data Sheet Premium ASA FormFutura
  36. Technical Data Sheet Premium PETG Flame Retardant FormFutura
  37. Technical Data Sheet Kratos PC FormFutura
  38. Technical Data Sheet Kratos PC CF10 FormFutura
  39. Moisture Ruins Prints – Here's How to Fix It! FormFutura blog
  40. Wet Filament? Here's How to Fix It. (updated 2026-08-25) MatterHackers
  41. NylonX Carbon Fiber PA12 Filament MatterHackers
  42. How to Dry 3D Printer Filament — PLA, PETG, TPU, ABS & Nylon Drying Temps (2026-02-28) Overture 3D blog
  43. Filament Drying Guide Overture 3D Wiki
  44. PolyLite™ PLA Polymaker Wiki
  45. Panchroma™ Silk PLA Polymaker Wiki
  46. PLA-CF Polymaker Wiki
  47. PolyLite™ PETG Polymaker Wiki
  48. Polylite™ ABS Polymaker Wiki
  49. Polymaker™ ASA Polymaker Wiki
  50. PolyFlex™ TPU95 Polymaker Wiki
  51. PolyFlex™ TPU90 Polymaker Wiki
  52. PolyLite™ PC Polymaker Wiki
  53. PolyMide™ CoPA Polymaker Wiki
  54. Drying filament Prusa Knowledge Base
  55. Prusament PLA Prusament (Prusa Research)
  56. Prusament PETG Prusament (Prusa Research)
  57. Prusament TPU 95A Prusament (Prusa Research)
  58. Prusament ASA Prusament (Prusa Research)
  59. Prusament PC Blend Prusament (Prusa Research)
  60. Prusament PC Blend Carbon Fiber Prusament (Prusa Research)
  61. Prusament PA11 (Nylon) Carbon Fiber Prusament (Prusa Research)
  62. Prusament PP Carbon Fiber Prusament (Prusa Research)
  63. Prusament PEI 1010 Prusament (Prusa Research)
  64. Siraya Tech Flex TPU 95A Filament (TDS page) Siraya Tech
  65. Siraya Tech Fibreheart PET-CF TDS Siraya Tech
  66. How to Dry 3D Printer Filament at Home (2026-01-13) Siraya Tech blog
  67. SUNLU Wiki - General Filaments SUNLU
  68. SUNLU Wiki - Esthetic Filaments SUNLU
  69. SUNLU Wiki - Functional Filaments SUNLU
  70. SUNLU Wiki - Engineering Filaments SUNLU